Chemical/mechanical polishing can be used to polish the rough surface of diamond films prepared by chemical vapor deposition (CVD). In this paper, a mixture of oxidizing agents (LiNO3+KNO3) has been introduced to improve the material removal rate and the surface roughness in chemical/mechanical polishing because of its lower melting point. It had been shown that by using this mixture the surface roughness Ra(arithmetic average roughness) could be reduced from 817 to 0.4 Am in 3 h of polishing, and the material removal rate can reach 1.72.3 mg/cm2/h at the temperature of 623 K. Pure aluminium is compared with cast iron as the contact disk material in the polishing. Although the material removal rate of aluminiumdisk is lower than that of cast iron, it can eliminate the carbon contamination from the contact disk to the surface of diamond films, and facilitate the analysis of the status of diamond in the chemical/mechanical polishing. The surface character and material removal rate of diamond films under different polishing pressure and rotating speed have also been studied. Graphite and amorphous carbon were detected on the surface of polished diamond films by Raman spectroscopy. It has been found that the oxidization and graphitization combined with mechanical cracking account for the high material removal rate in chemical/mechanical polishing of diamond films. D 2005 Elsevier B.V. All rights reserved.

全文请访问: 扫描探针显微镜(SPM/AFM/STM)
相关产品
相关解决方案
热门解决方案
最新解决方案
在线留言
官方微信

仪器网微信服务号

扫码获取最新信息


仪器网官方订阅号

扫码获取最新信息

在线客服

咨询客服

在线客服
工作日:  9:00-18:00
联系客服 企业专属客服
电话客服:  400-822-6768
工作日:  9:00-18:00
订阅商机

仪采招微信公众号

采购信息一键获取海量商机轻松掌控